CWN logo COIL WINDING NEWS Industry news for coil winding professionals
Coiltech Germany 2027, 17-18 March 2027, Messe Augsburg - international coil and winding exhibitionAdvertisement
Article

Advances in High-Temperature Magnet Wire Insulation

By Tobias Buban | 25 Nov 2026

Motors and drives are asking more of the winding. Higher power density and inverter duty push the wire to run hotter, so the enamel has to be better.

Polyimide family

A 2024 review in the journal Materials describes polyimides, polyamide-imides, polyetherimides and polyesterimides as important high-performance polymers, all with imide rings. It says polyimide has excellent thermal stability, and that at 250 C the service life of polyimide-enamelled wire can exceed 10,000 hours. It reports a hybrid polyimide film with a heat-resistance grade above 240 C. Polyimide paints are also used as impregnation varnish, topcoats and anti-corona paint on large high-voltage motors.

PEEK

The review describes polyetheretherketone, PEEK, as a semi-crystalline engineering plastic with high temperature, chemical and oxidation resistance, and it lists excellent strength and rigidity, self-lubricating properties, fire resistance and stable physical structure among its features. Those mechanical properties matter for wire that is bent and formed in a winding process. A maker of PEEK for magnet wire insulation says its polymer gives stable operation from -40 C up to 260 C and targets magnet wire for high-voltage e-motors. That is a manufacturer's claim about its own material, so check the data sheet and test results for your wire.

Limits

The review says the tolerance temperature of existing organic insulation does not exceed 250 C, and hybridisation and branching can add only tens of degrees, still below 300 C. It puts the current limit of organic high-temperature insulation for electromagnetic wire at no more than 285 C. The reason it gives is thermal degradation of the polymer molecules. Going beyond that would need different materials.

Supply side

A magnet wire maker says capacity for 200 C and higher grades is tighter than for standard 130 to 180 C wire, since high-temperature enamels need more passes and slower line speeds, and the demand from inverter-duty and EV traction motors is growing. It advises booking capacity earlier and expecting longer sample cycles. This is one maker's view of the market.

Design for substitution

The same maker suggests that if a design can accept either a 180 C or a 200 C build, the engineering work done once at design stage gives a substitution route when one family is congested. Decide this early, with test data for both builds, since changing the thermal class late means requalifying the winding and the varnish.

What to check

  1. Thermal class of the wire and of the whole insulation system. See motor winding temperature classes.
  2. Test data for the wire, not only the polymer.
  3. Flexibility and adhesion after bending and forming.
  4. Voltage and partial discharge needs. See corona-resistant magnet wire.
  5. Lead time for the grade.

Frequently asked questions

What is the main material family?

Polyimide and related imide polymers such as polyamide-imide.

What is PEEK used for?

As an extruded insulation for magnet wire in high-voltage motors, per its maker.

How hot can organic insulation go?

A 2024 review says current materials are limited to about 285 C.

Is polyimide enamel long-lived?

The review says over 10,000 hours at 250 C.

Why check lead times?

High-temperature grades may have tighter capacity.

Sources

  • Materials 2024, 17(10):2258: research progress in high-temperature-resistant electromagnetic wire (polyimide, PEEK, limits of organic insulation)
  • Victrex: XPI PEEK polymer for magnet wire insulation in high-voltage e-motors (manufacturer literature)
  • Huaya Magnet Wire: magnet wire supply chain in 2026, copper prices, capacity and lead times (manufacturer article, 8 Oct 2026)